anvilfire logo (c) 1998 by P.J. Dempsey
anvilfire home
anvilfire! News

Blacksmithing News and Events

Cyber Smiths International Logo
Cyber Smiths Int.
Edition 42 - Page 7 of 25 September 30, 2008

SOFA 2008 - Thermite Welding RR-Rail

The mold assembly
The red sand mold parts are held in place with a steel casing.
The mold assembly
Sealing the mold
The mold assembly
The entire brick of clay is used to seal the mold.
The mold assembly
Retrieving mold brackets from the first weld which is nearly cooled. Preheat torch setup on second weld.
The mold assembly
The disposable crucible prior to filling.

. . much more . .
1  2  3  4  5  6  7 
8  9  10  11  12 
13  14  15  16  17 
18  19  20  21  22 
23  24  25 











Online Metals Sales Logo

Page 1   Page 2   Page 3   Page 4   Page 5   Page 6   [42-7]   Page 8   Page 9   Page 10   NEWS HOME
September 30, 2008
SOFA CONF 2008
Comments to: Editor at anvilfire.com
Copyright © 2008 by Jock Dempsey
Page Counter   -   Cumulitive News