Dimensions for Standard Tongs
 |
Capacity In. |
A |
B |
C |
D |
E |
F |
G |
H |
I |
K |
L |
Rivet |
0 - 1/8 |
5/8 |
3/8 |
1/4 |
5/8 |
1/16 |
2-1/8 |
1/2 |
5/16 |
5/16 |
1/4 |
14 |
1/4 |
3/16 - 5/16 |
3/4 |
7/16 |
5/16 |
5/8 |
1/16 |
2-1/4 |
9/16 |
5/16 |
5/16 |
1/4 |
15 |
1/4 |
3/8 - 7/16 |
7/8 |
1/2 |
5/16 |
3/4 |
1/16 |
2-1/2 |
5/8 |
3/8 |
3/8 |
5/16 |
16 |
5/16 |
1/2 - 5/8 |
1 |
9/16 |
3/8 |
7/8 |
3/32 |
2-3/4 |
11/16 |
7/16 |
3/8 |
5/16 |
18 |
3/8 |
3/4 - 7/8 |
1-1/8 |
5/8 |
3/8 |
1 |
5/32 |
3 |
3/4 |
1/2 |
7/16 |
3/8 |
20 |
7/16 |
1 - 1-1/8 |
1-1/4 |
11/16 |
7/16 |
1-1/8 |
3/16 |
3-1/4 |
13/16 |
9/16 |
1/2 |
7/16 |
22 |
1/2 |
1-1/4 - 1-3/8 |
1-3/8 |
3/4 |
1/2 |
1-1/8 |
1/4 |
3-1/2 |
7/8 |
9/16 |
1/2 |
7/16 |
24 |
9/16 |
1-1/2 - 1-5/8 |
1-1/2 |
3/4 |
1/2 |
1-1/4 |
3/8 |
3-3/4 |
1 |
5/8 |
5/8 |
1/2 |
26 |
5/8 |
1-3/4 - 1-7/8 |
1-5/8 |
13/16 |
9/16 |
1-3/8 |
7/16 |
4 |
1-1/16 |
11/16 |
5/8 |
1/2 |
28 |
5/8 |
2 |
1-3/4 |
7/8 |
5/8 |
1-1/2 |
7/16 |
4-1/4 |
1-1/8 |
3/4 |
11/16 |
1/2 |
30 |
11/16 |
Machinery's Handbook 1st - 23rd edition and 27th Edition CD used with permission. |
 |
Capacity In. |
A |
B |
C |
D |
E |
F |
G |
H |
I |
L |
Rivet |
1/4 - 5/16 |
5/8 |
1/2 |
7/16 |
5/16 |
1/8 |
1 |
1/2 |
5/16 |
1/4 |
14 |
1/4 |
3/8 - 7/16 |
3/4 |
9/16 |
1/2 |
5/16 |
3/16 |
1-1/8 |
9/16 |
5/16 |
1/4 |
16 |
5/16 |
1/2 - 5/8 |
7/8 |
5/8 |
9/16 |
3/8 |
1/4 |
1-1/4 |
5/8 |
3/8 |
5/16 |
18 |
3/8 |
3/4 - 7/8 |
1 |
3/4 |
5/8 |
7/16 |
3/8 |
1-1/2 |
3/4 |
3/8 |
5/16 |
20 |
7/16 |
1 - 1-1/8 |
1-1/8 |
7/8 |
11/16 |
1/2 |
1/2 |
1-3/4 |
7/8 |
3/8 |
5/16 |
20 |
1/2 |
1-1/4 - 1-3/8 |
1-1/4 |
1 |
3/4 |
9/16 |
5/8 |
2 |
1 |
7/16 |
3/8 |
22 |
1/2 |
1-1/2 - 1-3/4 |
1-3/8 |
1-1/8 |
7/8 |
5/8 |
3/4 |
2-1/8 |
1-1/8 |
1/2 |
3/8 |
24 |
9/16 |
1-7/8 - 2-1/8 |
1-3/8 |
1-3/16 |
15/16 |
11/16 |
1 |
2-1/4 |
1-1/4 |
1/2 |
3/8 |
26 |
5/8 |
2-1/4 - 2-1/2 |
1-1/2 |
1-1/4 |
1 |
3/4 |
1-1/8 |
2-1/2 |
1-1/2 |
9/16 |
7/16 |
28 |
5/8 |
2-5/8 - 2-7/8 |
1-1/2 |
1-5/16 |
1-1/16 |
3/4 |
1-1/4 |
2-3/4 |
1-3/4 |
9/16 |
7/16 |
30 |
3/4 |
3 - 3-1/4 |
1-5/8 |
1-3/8 |
1-1/8 |
3/4 |
1-1/2 |
3 |
2 |
5/8 |
1/2 |
32 |
3/4 |
3-1/2 - 3-3/4 |
1-3/4 |
1-1/2 |
1-1/4 |
3/4 |
1-3/4 |
3-1/4 |
2-1/4 |
5/8 |
1/2 |
34 |
3/4 |
4 - 4-1/4 |
2 |
1-5/8 |
1-5/16 |
13/16 |
2 |
3-1/4 |
2-1/2 |
11/16 |
9/16 |
36 |
3/4 |
4-1/2 - 4-3/4 |
2-1/8 |
1-5/8 |
1-5/16 |
13/16 |
2-1/8 |
3-1/4 |
2-3/4 |
11/16 |
9/16 |
38 |
3/4 |
5 |
2-1/4 |
1-3/4 |
1-3/8 |
7/8 |
2-1/4 |
3-1/2 |
3-1/4 |
3/4 |
5/8 |
40 |
7/8 |
Machinery's Handbook 1st - 23rd edition and 27th Edition CD used with permission. |
Copyright © 1914 - 2004 by Industrial Press - HTML Copyright © 2004 Jock Dempsey
Webmaster email: webmaster
web address: www.anvilfire.com
|
|
|
Dimensions for Standard Tongs
Copyright © 1914 - 2004 by Industrial Press - HTML Copyright © 2004 Jock Dempsey
Webmaster email: webmaster web address: www.anvilfire.com