International Technical Ceramics products sold by Dempsey's Forge
|
ITC-100 HT Ceramic Coating
- Surface Preparation
- Remove all loose and weakened fiber, bricks, debris, particles, dust and grease from interior walls, door, crown, floor and grooves behind electrical elements.
Immediately before applying ITC-100 HT, dampen surface by spraying lightly with water.
- Mixing - Dilution
- To 1 part ITC-100 HT add 1/2 part water by volume and mix well.
Power mixing is required for large quantities.
Mixing then letting set for a few hours or overnight then mixing again produces a smooth mixture.
- Applying
- Spray large surfaces using a texture paint system of the type used for ceilings.
A canister type spray gun with nozzle suitable for ceramics can be used for medium size surfaces.
Agitate as necessary to prevent settling.
For small areas a brush can be used.
Generally an inexpensive 1" (25mm) brush is suitable but for tight places a large artist's paint brush of about 1/2" (12mm) works well.
When brushing onto ceramic fiber two coats are usually needed.
The first coat may be fired briefly prior to second coat.
|
ITC-296 A High Purity Ceramic Coating
- Surface Preparation
- Apply ITC-100 HT or other ITC products according to instructions.
Fire thoroughly (ITC recommends two or three times) before applying ITC-296A.
- Mixing - Dilution
- To 1 part ITC-100 HT add 1/2 part water by volume and mix well.
Power mixing is required for large quantities.
Mixing then letting set for a few hours or overnight then mixing again produces a smooth mixture.
- Applying
- Spray large surfaces using a texture paint system of the type used for ceilings.
A canister type spray gun with nozzle suitable for ceramics can be used for medium size surfaces.
Agitate as necessary to prevent settling.
For small areas a brush can be used.
Generally an inexpensive 1" (25mm) brush is suitable but for tight places a large artist's paint brush of about 1/2" (12mm) works well.
A thin top coat of a maximum of 1/32" (.08 mm) is all that is necessary.
|
ITC-213 Ceramic Coating for Metals
- Surface Preparation
- Remove all loose rust layers, grease, dirt and molten metal or scale buildup.
If possible roughen the surface by using a file or hacksaw blade.
Sandblasting is not recommended but is not detrimental.
Wash surface with a 1 : 1 solution of liquid Chlorox
bleach and water. DO NOT use solvent based degreasers.
- Mixing - Dilution
- To 1 part ITC-213 add 1/3 part water by volume and mix well.
Power mixing is required for large quantities.
Mixing then letting set for a few hours or overnight then mixing again produces a smooth mixture.
- Applying
- The best results are obtained by using a paint edger or a piece of cloth dipped in the
ITC-213 and then vigorously rubbing the coating onto the surface as thinly as possible.
A thin top coat is all that is necessary.
|
International Technical Ceramics LLC, Southlake, TX 76092, USA
DEMPSEY'S FORGE / anvilfire.com, Boonville, NC, USA : 336-367-3499
Copyright © 2011 anvilfire.com
|
|