At least one is! "Sister" is on the way! At left Chuck is making splinters with the West Coast Junk Yard Hammer on its maiden test! West Coast JYH photos by Grant Sarver
Below, the parts for the East Coast JYH! |
|||
![]() Now THAT'S HOT! A good soaking white heat is just the thing to test the JYH! |
![]() |
|||
$20 - 235 Chevy engine block with crank $25 - Scrap steel anvil plate $20 - 1 HP motor $36 - Springs $18 - 18 inch v-belt pulley (Could be wood) $5 - Railroad rail free - Bolts, iron, shop junk $124 - TOTAL |
$50 - Axel from full sized GM wagon $40 - (2) NEW Shocks $25 - (1) 1/2 HP motor, 2nd 3/4 HP motor NA $50 - Estimated value of 600 pounds scrap steel $1 - Metal pan for drum guard - free = V8 engine block, engine step pulley & belt $166 - Spent to date : Est. Wt. 1200 pounds |
|||
|