Capacity In. | A | B | C | D | E | F | G | H | I | K | L | Rivet |
0 - 1/8 | 5/8 | 3/8 | 1/4 | 5/8 | 1/16 | 2-1/8 | 1/2 | 5/16 | 5/16 | 1/4 | 14 | 1/4 |
3/16 - 5/16 | 3/4 | 7/16 | 5/16 | 5/8 | 1/16 | 2-1/4 | 9/16 | 5/16 | 5/16 | 1/4 | 15 | 1/4 |
3/8 - 7/16 | 7/8 | 1/2 | 5/16 | 3/4 | 1/16 | 2-1/2 | 5/8 | 3/8 | 3/8 | 5/16 | 16 | 5/16 |
1/2 - 5/8 | 1 | 9/16 | 3/8 | 7/8 | 3/32 | 2-3/4 | 11/16 | 7/16 | 3/8 | 5/16 | 18 | 3/8 |
3/4 - 7/8 | 1-1/8 | 5/8 | 3/8 | 1 | 5/32 | 3 | 3/4 | 1/2 | 7/16 | 3/8 | 20 | 7/16 |
1 - 1-1/8 | 1-1/4 | 11/16 | 7/16 | 1-1/8 | 3/16 | 3-1/4 | 13/16 | 9/16 | 1/2 | 7/16 | 22 | 1/2 |
1-1/4 - 1-3/8 | 1-3/8 | 3/4 | 1/2 | 1-1/8 | 1/4 | 3-1/2 | 7/8 | 9/16 | 1/2 | 7/16 | 24 | 9/16 |
1-1/2 - 1-5/8 | 1-1/2 | 3/4 | 1/2 | 1-1/4 | 3/8 | 3-3/4 | 1 | 5/8 | 5/8 | 1/2 | 26 | 5/8 |
1-3/4 - 1-7/8 | 1-5/8 | 13/16 | 9/16 | 1-3/8 | 7/16 | 4 | 1-1/16 | 11/16 | 5/8 | 1/2 | 28 | 5/8 |
2 | 1-3/4 | 7/8 | 5/8 | 1-1/2 | 7/16 | 4-1/4 | 1-1/8 | 3/4 | 11/16 | 1/2 | 30 | 11/16 | Machinery's Handbook 1st - 23rd edition and 27th Edition CD used with permission. |
![]() |
|||||||||||
Capacity In. | A | B | C | D | E | F | G | H | I | L | Rivet |
1/4 - 5/16 | 5/8 | 1/2 | 7/16 | 5/16 | 1/8 | 1 | 1/2 | 5/16 | 1/4 | 14 | 1/4 |
3/8 - 7/16 | 3/4 | 9/16 | 1/2 | 5/16 | 3/16 | 1-1/8 | 9/16 | 5/16 | 1/4 | 16 | 5/16 |
1/2 - 5/8 | 7/8 | 5/8 | 9/16 | 3/8 | 1/4 | 1-1/4 | 5/8 | 3/8 | 5/16 | 18 | 3/8 |
3/4 - 7/8 | 1 | 3/4 | 5/8 | 7/16 | 3/8 | 1-1/2 | 3/4 | 3/8 | 5/16 | 20 | 7/16 |
1 - 1-1/8 | 1-1/8 | 7/8 | 11/16 | 1/2 | 1/2 | 1-3/4 | 7/8 | 3/8 | 5/16 | 20 | 1/2 |
1-1/4 - 1-3/8 | 1-1/4 | 1 | 3/4 | 9/16 | 5/8 | 2 | 1 | 7/16 | 3/8 | 22 | 1/2 |
1-1/2 - 1-3/4 | 1-3/8 | 1-1/8 | 7/8 | 5/8 | 3/4 | 2-1/8 | 1-1/8 | 1/2 | 3/8 | 24 | 9/16 |
1-7/8 - 2-1/8 | 1-3/8 | 1-3/16 | 15/16 | 11/16 | 1 | 2-1/4 | 1-1/4 | 1/2 | 3/8 | 26 | 5/8 |
2-1/4 - 2-1/2 | 1-1/2 | 1-1/4 | 1 | 3/4 | 1-1/8 | 2-1/2 | 1-1/2 | 9/16 | 7/16 | 28 | 5/8 |
2-5/8 - 2-7/8 | 1-1/2 | 1-5/16 | 1-1/16 | 3/4 | 1-1/4 | 2-3/4 | 1-3/4 | 9/16 | 7/16 | 30 | 3/4 |
3 - 3-1/4 | 1-5/8 | 1-3/8 | 1-1/8 | 3/4 | 1-1/2 | 3 | 2 | 5/8 | 1/2 | 32 | 3/4 |
3-1/2 - 3-3/4 | 1-3/4 | 1-1/2 | 1-1/4 | 3/4 | 1-3/4 | 3-1/4 | 2-1/4 | 5/8 | 1/2 | 34 | 3/4 |
4 - 4-1/4 | 2 | 1-5/8 | 1-5/16 | 13/16 | 2 | 3-1/4 | 2-1/2 | 11/16 | 9/16 | 36 | 3/4 |
4-1/2 - 4-3/4 | 2-1/8 | 1-5/8 | 1-5/16 | 13/16 | 2-1/8 | 3-1/4 | 2-3/4 | 11/16 | 9/16 | 38 | 3/4 |
5 | 2-1/4 | 1-3/4 | 1-3/8 | 7/8 | 2-1/4 | 3-1/2 | 3-1/4 | 3/4 | 5/8 | 40 | 7/8 | Machinery's Handbook 1st - 23rd edition and 27th Edition CD used with permission. |