Blacksmith Anvil Hardy (square) Hole Sizes |
Brand |
Anvil Size/Weight in Pounds |
50 |
100 |
120 |
150 |
160 |
180 |
200 |
250 |
350 |
500 |
600 |
750 |
Arm & Hammer |
3/4 |
7/8 |
1 |
1-1/16 |
1-1/16 |
1-1/8 |
1-1/8 |
1-1/8 |
1-1/4 |
1-3/8 |
|
|
Brooks |
5/8 |
3/4 |
7/8 |
1-1/4 |
1-1/4 |
|
1-1/4 |
|
|
|
|
|
Columbian |
3/4 |
7/8 |
1 |
1 |
|
|
1-1/8 |
1-1/4 |
1-3/8 |
1-1/2 |
1-1/2 |
|
Eagle |
5/8 |
3/4 |
3/4 |
7/8 |
1 |
1 |
1-1/8 |
1-1/4 |
1-3/8 |
1-1/2 |
1-1/2 |
1-5/8 |
Hay-Budden |
3/4 |
3/4 |
7/8 |
7/8 |
|
1 |
1-1/8 |
1-1/8 |
1-1/4 |
1-1/2 |
1-3/4 |
|
Vulcan |
1/2 |
3/4 |
|
7/8 |
1 |
1-1/4 |
1-1/4 |
|
|
|
|
Kohlswa A1 |
22 mm |
22 mm |
22 |
|
25 mm |
|
32 mm |
35 |
35 |
|
|
|
Kohlswa B27 |
20 mm |
23 |
25 |
27 |
28 |
29 |
|
32 |
36 |
41 |
|
|
Paragon |
5/8 |
7/8 |
1 |
1 |
1 |
1-1/8 |
1-1/4 |
1-3/8 |
1-3/8 |
1-1/2 |
|
|
Peter Wright |
5/8 |
3/4 |
7/8 |
1 |
1 |
1 |
1-1/8 |
1-1/4 |
1-3/8 |
1-1/2 |
1-1/2 |
|
Peddinghaus |
3/4 |
1 |
|
|
|
|
Euroanvils |
|
|
|
|
1 |
|
|
Nimba |
|
|
1 |
|
|
|
Due to anvil weights not all being in the same increments and manufacturers not making the same range of product, this survey of sizes and may have some inaccuracies. |