Blacksmith Anvil Hardy (square) Hole Sizes
Brand Anvil Size/Weight in Pounds
50 100 120 150 160 180 200 250 350 500 600 750
Arm & Hammer 3/4 7/8 1 1-1/16 1-1/16 1-1/8 1-1/8 1-1/8 1-1/4 1-3/8    
Brooks 5/8 3/4 7/8 1-1/4 1-1/4   1-1/4          
Columbian 3/4 7/8 1 1     1-1/8 1-1/4 1-3/8 1-1/2 1-1/2  
Eagle 5/8 3/4 3/4 7/8 1 1 1-1/8 1-1/4 1-3/8 1-1/2 1-1/2 1-5/8
Hay-Budden 3/4 3/4 7/8 7/8   1 1-1/8 1-1/8 1-1/4 1-1/2 1-3/4  
Vulcan 1/2 3/4   7/8 1-1/4 1-1/4        
Kohlswa A1 22 mm 22 mm 22   25 mm   32 mm 35 35      
Kohlswa B27 20 mm 23 25 27 28 29   32 36 41    
Paragon 5/8 7/8 1 1 1   1-1/8 1-1/4 1-3/8 1-3/8 1-1/2    
Peter Wright 5/8 3/4 7/8 1 1 1 1-1/8 1-1/4 1-3/8 1-1/2 1-1/2  
Peddinghaus 3/4 1        
Euroanvils         1    
Nimba     1      
Due to anvil weights not all being in the same increments and manufacturers not making the same range of product, this survey of sizes and may have some inaccuracies. Data compiled for anvilfire.com Copyright © 2011 Jock Dempsey